Restock alerts are coming soon. For now, check back or ask us at [email protected]. We'll email you when it's back in stock. We'll email and text you when it's back in stock. Restock alerts are off for this item. It stays on My List. That didn't save. Try again. That didn't go through. Try again. Check the mobile number and try again. Tick the box to get texts. Save it to a list first. Good news: it's in stock now. Turn off an alert you no longer need, then try again. Couldn't save in this browser. Ask us when it's due back: [email protected]

Description

EarthCoat ElectroKing Electrocleaning Concentrate Powder is a versatile soak cleaner and electrocleaner formulated for jewelry and industrial substrates. Mix the powder concentrate with water and clean by simple immersion or by electrocleaning with a rectifier. Effective on common shop soils and compatible with a wide range of metals used in jewelry fabrication and plating lines.

Features

  • Dual-mode use: immersion soak cleaning or electrocleaning with a rectifier
  • Economical powder concentrate — easy to mix, make up, and maintain
  • Compatible with white metal, copper, brass, steel, silver, gold, bronze, nickel, and zinc
  • Sold in a 2 lb (0.91 kg) container

Specifications

Form Powder concentrate
Container Size 2 lb (0.91 kg)
Mix Ratio 1/4 lb powder per gallon of water (approx. 30 g/L)
Bath Temperature 140 °F (60 °C)
Electrocleaning Voltage 2–6 volts
Electrocleaning Time 15–60 seconds
Anode Material Stainless steel
Soak Cleaning Time 1–5 minutes at 140 °F (60 °C)

Basic Setup

  1. Heat water to approximately 140 °F (60 °C), then add the measured ElectroKing powder and stir until fully dissolved.
  2. For electrocleaning, connect the workpiece negative (–) and the stainless steel anode positive (+); clean for 15–60 seconds at 2–6 volts.
  3. For soak cleaning without a rectifier, immerse parts for 1–5 minutes at 140 °F (60 °C).
  4. Rinse thoroughly after cleaning before proceeding to activation or plating.

Notes

  • Use in a well-ventilated area. Wear gloves, safety goggles, and a protective apron.
  • Do not add powder to water heated above 140 °F (60 °C).
  • Avoid prolonged skin contact.
  • Do not mix with Activator-T below 100 °F (32 °C).

Specifications

Brand
Cohler
Part #
145.730
Type
Plating Solutions
Dimensions
8 in x 3.75 in x 3.75 in
Form
Powder concentrate
Container Size
2 lb (0.91 kg)
Mix Ratio
1/4 lb powder per gallon of water (approx. 30 g/L)
Bath Temperature
140 °F (60 °C)
Electrocleaning Voltage
2–6 volts
Electrocleaning Time
15–60 seconds
Anode Material
Stainless steel
Soak Cleaning Time
1–5 minutes at 140 °F (60 °C)

Documents

Specs, manuals, and certificates for this product. All files open in a new tab.

California Prop 65 Warning California Prop 65 Warning:
Cancer and Reproductive Harm. www.P65warnings.ca.gov.

Reviews · 1

This product has 1 review.

Read & write reviews ↓
  • 5 stars: 1 (100%)
  • 4 stars: 0 (0%)
  • 3 stars: 0 (0%)
  • 2 stars: 0 (0%)
  • 1 star: 0 (0%)
D
David Worcester
Great cleaner with low cost shipping

This is a very effective cleaner and brightener, and a real plus is that it ships normally; all other electrocleaners that I'm aware of require expensive hazardous materials shipping. I use it on Argentium 960 for every piece that I produce - the bulk of my work. This has been found to enhance Argentium silver's tarnish resistance. I use six volts for 75 seconds. I just discovered that this can also be used in the ultrasonic, but I love the Ottosonic Cleaner (123.616) which I buy by the gallon and doubt that I will change using that in the ultrasonic cleaner prior to electrocleaning.