Skip to content

Ultra White 9K-18K Stone-In-Place Nickel Alloy

Part # 846-982 4 In Stock Weight <0.1 lb / <5 g
Current price $39.05

Availability Sold out

Restock alerts are coming soon. For now, check back or ask us at [email protected]. We'll email you when it's back in stock. We'll email and text you when it's back in stock. Restock alerts are off for this item. It stays on My List. That didn't save. Try again. That didn't go through. Try again. Check the mobile number and try again. Tick the box to get texts. Save it to a list first. Good news: it's in stock now. Turn off an alert you no longer need, then try again. Couldn't save in this browser. Ask us when it's due back: [email protected]

Description

Ultra White 9K–18K Stone-In-Place Investment Casting Master Alloy is formulated for excellent fluidity during casting and fabrication applications. Contains no gold. Sold by the troy ounce (20 pennyweights / 31.1 grams).

Features

  • Engineered for stone-in-place investment casting with excellent metal fluidity
  • Compatible with 9K through 18K gold formulations when pre-alloyed with fine gold
  • Suitable for both casting and fabrication applications
  • Contains no gold — a true master alloy for alloying to karat
  • Gypsum bonded investment recommended for best results
  • Fluoride-based investment removers recommended for silicon oxide coating removal

Specifications

Composition Cu 53%, Ag 20%, Zn 10%, Ni 17% (plus proprietary metals; may also contain silicon and deoxidizers)
Contains Gold No
Sold By Troy ounce (20 pennyweights / 31.1 grams)
Pre-Alloying Temperature (9K–18K) 1050°C – 1060°C / 1922°F – 1940°F
Casting Temp – 10K Alloyed Grain 960°C – 980°C / 1760°F – 1796°F
Casting Temp – 14K Alloyed Grain 985°C – 1005°C / 1805°F – 1841°F
Casting Temp – 18K Alloyed Grain 980°C – 1000°C / 1796°F – 1832°F
Flask Temperature 540°C – 675°C / 1004°F – 1247°F (varies by flask size, karat, and jewelry type)
Quench Time 15–25 minutes

Notes

  • Pre-alloying with fine gold using aggressive stirring and fluxing is recommended to ensure a uniform mixture.
  • Use very little boric acid flux. Do not use carbon flux such as soda ash or saltpeter. No flux is needed in a bottom-pour automatic casting unit.
  • To calculate the weight of metal needed (in grams), multiply density (g/cc) by the weight of wax (grams), then add 10% for the button.
  • Avoid aggressive acids for investment removal — use fluoride-based removers to prevent stress corrosion and surface damage.
  • Recommended scrap mix: 60% fresh, 40% scrap. Note that white gold alloy has approximately one-third the reusability of yellow gold alloys.
  • Melt temperature may vary depending on the type of casting unit used.
  • Proprietary metals are present in the formulation and are not fully disclosed in the composition data.

Specifications

Brand
Otto Frei
Part #
846-982
Type
Alloys
Dimensions
2 in x 2 in x 0.5 in
Composition
Cu 53%, Ag 20%, Zn 10%, Ni 17% (plus proprietary metals; may also contain silicon and deoxidizers)
Contains Gold
No
Sold By
Troy ounce (20 pennyweights / 31.1 grams)
Pre-Alloying Temperature (9K–18K)
1050°C – 1060°C / 1922°F – 1940°F
Casting Temp – 10K Alloyed Grain
960°C – 980°C / 1760°F – 1796°F
Casting Temp – 14K Alloyed Grain
985°C – 1005°C / 1805°F – 1841°F
Casting Temp – 18K Alloyed Grain
980°C – 1000°C / 1796°F – 1832°F
Flask Temperature
540°C – 675°C / 1004°F – 1247°F (varies by flask size, karat, and jewelry type)
Quench Time
15–25 minutes

Documents

Specs, manuals, and certificates for this product. All files open in a new tab.

California Prop 65 Warning California Prop 65 Warning:
Cancer and Reproductive Harm. www.P65warnings.ca.gov.

Reviews

No reviews yet. Be the first to share your experience with this product.

Write a review ↓